再生绿色环保PP料,符合ROHS2.0,无气味,比重0.98.良好的加工性能,成型无料花。物性参考如下:
产 品 物 性 表 PROPERTY TABLE | |||||
品名Material: | PP | 型号Grade: | 绿色PP | ||
性能特点Feature: | 绿色 | 用途Application: | |||
性能 Properties | 测试项目 Test Item | 标准方法 Standard Method | 测试条件 Test Condition | 数 值 Values | 单位 Unit |
熔指 Melt Index | GB/T 3682-2000 | 230℃,2.16kg | 2.7 | g/10min | |
比重Specific Gravity | ASTM D792 | 0.98 | g/cm3 | ||
硬度Hardness | ASTM D2240 | Shore D | 60 | D | |
力学性能 Mechanical | 拉伸强度Tensile Strength | ASTM D638 | 5mm/min | 15.02 | Mpa |
断裂伸长率Elongation AT Break | ASTM D638 | 58.66 | % | ||
弹性模量Flexural Modulus | ASTM D2240 | 425.88 | Mpa | ||
IZOD冲击强度 Impact Strength,IZOD Notched | ASTM D256 | 23℃,干态 | 40.35 | J/M | |
热性能Themal | 热变形温度Distortion Temperature | ASTM D648 | 0.45MPa | ━ | ℃ |
ASTM D648 | 1.82MPa | ━ | ℃ | ||
电气性能 Electical | 体积电阻率Volume Resistivity | ASTM D257 | ━ | Ω.cm | |
电击穿强度Electric Breakdown Strength | ASTM D149 | ━ | KV | ||
可燃性 Flamblity | 阻燃性Ignition Resistance Flammability | UL94 | 1.6mm | ━ | |
*以上数据为测试典型值,仅作参考之用.所有数据是我方实验所得的真实数据并相信其准确性,但不能保证可引伸至使用者,使用者应自行测试加以确认。 | |||||
预处理及成型条件参考Pretreament and molding conditions | |||||
机筒温度Barrel temperature | 一段 Part 1 | 二段Part2 | 三段Part3 | 射嘴 Nozzle | |
200 | 200 | 195 | 195 | ||
射出时间Injection speed | 3S | 保压 Holding time | 1 | 模温mould temperature | 70~80℃ |
干燥处理方式Drying | 热风干燥 | 温度Temperature | 100℃ | 时间Time | 4H |
是否需后处理Molded treatment | 否 | 处理方式Method | 处理时间Time | ||
备注: |