| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 吸水率 | 24hr | ASTM D570 | 0.33 | % |
| 收缩率 | MD | ASTM D955 | 0.25to0.45 | % |
| 密度 | - | ASTM D792 | 1.51 | g/cm³ |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 摩擦系数 | --5 | ASTM D3702 | 0.29 | - |
| 磨损因数 | 0.22MPa,4.1m/sec9 | ASTM D3702 | 35 | 10^-8mm³/N·m |
| 拉伸模量 | -- | ASTM D638 | 8830 | MPa |
| --2 | ASTM D1708 | 7790 | MPa | |
| 拉伸强度 | - | ASTM D638 | 117 | MPa |
| - | ASTM D1708 | 131 | MPa | |
| 伸长率 | 断裂 | ASTM D638 | 2.6 | % |
| 断裂2 | ASTM D1708 | 7.0 | % | |
| 弯曲模量 | 23°C | ASTM D790 | 7310 | MPa |
| 232°C | ASTM D790 | 5100 | MPa | |
| 弯曲强度 | 23°C | ASTM D790 | 208 | MPa |
| 232°C | ASTM D790 | 110 | MPa | |
| 压缩模量 | - | ASTM D695 | 4000 | MPa |
| 压缩强度 | - | ASTM D695 | 123 | MPa |
| 摩擦系数 | --4 | ASTM D3702 | 0.31 | - |
| --6 | ASTM D1894 | 0.15 | - | |
| --7 | ASTM D1894 | 0.050 | - | |
| 磨损因数 | 5.2MPa,0.38m/sec8 | ASTM D3702 | 1.4 | 10^-8mm³/N·m |
| 6.9MPa,0.38m/sec8 | ASTM D3702 | 14 | 10^-8mm³/N·m | |
| 3.4MPa,0.25m/sec9 | ASTM D3702 | 26 | 10^-8mm³/N·m | |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 线性热膨胀系数 | - | ASTM D696 | 2.5E-05 | cm/cm/°C |
| 热变形温度 | 1.8MPa,未退火 | ASTM D648 | 280 | °C |
| 导热系数 | - | ASTMC177 | 0.65 | W/m/K |
| 电气性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 表面电阻率 | - | ASTM D257 | 4E+17 | ohms |
| 体积电阻率 | - | ASTM D257 | 8E+15 | ohms·cm |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 悬臂梁缺口冲击强度 | - | ASTM D256 | 85 | J/m |
| 悬壁梁无缺口冲击强度 | - | ASTM D256 | 270 | J/m |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。