| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 特定体积 | - | ASTM D792 | 1.20 | cm³/g |
| 熔体质量流动速率 | 250°C/5.0kg | ASTMD1238 | 16 | g/10min |
| 收缩率 | MD:3.20mm | Internal Method | 0.80-1.0 | % |
| TD:3.20mm | Internal Method | 0.80-1.0 | % | |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 屈服 | - | ASTM D638 | 45.2 | Mpa |
| - | ASTM D638 | 48.8 | Mpa | |
| - | ISO 527-2/50 | 52.4 | Mpa | |
| 断裂 | - | ASTM D638 | 46.0 | Mpa |
| - | ASTM D638 | 47.4 | Mpa | |
| - | ISO 527-2/50 | 50.5 | Mpa | |
| 屈服 | - | ASTM D638 | 4.1 | % |
| - | ASTM D638 | 4.2 | % | |
| - | ISO 527-2/50 | 4.5 | % | |
| 断裂 | - | ASTM D638 | 110 | % |
| - | ASTM D638 | 1990 | Mpa | |
| - | ASTM D638 | 2020 | Mpa | |
| 断裂 | - | ASTM D638 | 120 | % |
| - | ISO 527-2/50 | 120 | % | |
| 50.0mm跨距 | - | ASTM D790 | 1900 | Mpa |
| - | ISO 178 | 2020 | Mpa | |
| - | ISO 178 | 78.9 | Mpa | |
| 屈服,50.0mm跨距 | - | ASTM D790 | 76.1 | Mpa |
| 断裂,50.0mm跨距 | - | ASTM D790 | 74.7 | Mpa |
| 断裂弯曲应变 | - | ISO 178 | 7.3 | % |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 0.45MPa,未退火,6.40mm | - | ASTM D648 | 115 | °C |
| 0.45MPa,未退火,64.0mm跨距 | - | ISO 75-2/Bf | 109 | °C |
| 1.8MPa,未退火,6.40mm | - | ASTM D648 | 97.0 | °C |
| 1.8MPa,未退火,64.0mm跨距 | - | ISO 75-2/Af | 90.2 | °C |
| 维卡软化温度 | - | ASTMD1525 | 123 | °C |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 硬度 | 邵氏D | ISO 868 | 79 | - |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| -40℃ | ASTM D256 | 370 | J/m | |
| -30°C | - | ASTM D256 | 490 | J/m |
| -20°C | - | ASTM D256 | 690 | J/m |
| -10°C | - | ASTM D256 | 700 | J/m |
| 0°C | - | ASTM D256 | 720 | J/m |
| 23°C | - | ASTM D256 | 760 | J/m |
| -40℃ | ISO 180/1A | 35 | kJ/m² | |
| -30°C | - | ISO 180/1A | 51 | kJ/m² |
| 23°C | - | ISO 180/1A | 63 | kJ/m² |
| 简支梁缺口冲击强度 | -30°C | ISO 179/1eA | 48 | kJ/m² |
| 23°C | ISO 179/1eA | 63 | kJ/m² |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。