| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 密度 | - | ASTM D792 | 1.82 | g/cm³ |
| 门尼粘度 | ML1+10,121°C | ASTM D1646 | 63 | MU |
| 弹性体 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 压缩永久变形 | 232°C,70hr | ASTM D395B | 37 | % |
| 拉伸强度 | 100%应变,23°C6 | ASTM D412 | 3.80 | MPa |
| 屈服,23°C6 | ASTM D412 | 9.50 | MPa | |
| 屈服,23°C7 | ASTM D412 | 12.5 | MPa | |
| 屈服,23°C9 | ASTM D412 | 14.3 | MPa | |
| 屈服,23°C10 | ASTM D412 | 13.1 | MPa | |
| 伸长率 | 断裂,23°C6 | ASTM D412 | 300 | % |
| 拉伸强度 | 屈服,23°C8 | ASTM D412 | 12.8 | MPa |
| 伸长率 | 断裂,23°C7 | ASTM D412 | 210 | % |
| 断裂,23°C8 | ASTM D412 | 210 | % | |
| 断裂,23°C9 | ASTM D412 | 210 | % | |
| 断裂,23°C10 | ASTM D412 | 210 | % | |
| 压缩永久变形 | 23°C,70hr | ASTM D395B | 7.0 | % |
| 200°C,70hr | ASTM D395 | 17 | % | |
| 拉伸强度 | 100%应变,23°C7 | ASTM D412 | 5.00 | MPa |
| 100%应变,23°C8 | ASTM D412 | 5.60 | MPa | |
| 100%应变,23°C9 | ASTM D412 | 5.50 | MPa | |
| 100%应变,23°C10 | ASTM D412 | 5.20 | MPa | |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 硬度 | 邵氏A,23°C3 | ASTM D2240 | 79 | - |
| 邵氏A,23°C4 | ASTM D2240 | 77 | - | |
| 邵氏A,23°C5 | ASTM D2240 | 76 | - | |
| 邵氏A,23°C | ASTM D2240 | 78 | - | |
| 邵氏A,23°C2 | ASTM D2240 | 76 | - |