| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 熔体质量流动速率 | 300°C/1.2kg | ASTM D1238 | 24 | g/10min |
| 熔体体积流动速率 | 300°C/1.2kg | ASTM D1238 | 22.0 | cm3/10min |
| 收缩率 | MD:3.20mm | Internal Method | 0.20-0.40 | % |
| TD:3.20mm | Internal Method | 0.30-0.50 | % | |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 断裂 | - | ISO 527-2/5 | 45.0 | Mpa |
| 屈服 | - | ASTM D638 | 4.1 | % |
| - | ISO 527-2/5 | 4.0 | % | |
| 断裂 | - | ASTM D638 | 6.9 | % |
| - | ISO 527-2/5 | 6.8 | % | |
| 50.0mm跨距 | - | ASTM D790 | 3600 | Mpa |
| - | ISO 178 | 4000 | Mpa | |
| - | ISO 178 | 108 | Mpa | |
| - | ISO 178 | 110 | Mpa | |
| 屈服,50.0mm跨距 | - | ASTM D790 | 104 | Mpa |
| 断裂,50.0mm跨距 | - | ASTM D790 | 102 | Mpa |
| - | ASTM D638 | 4000 | Mpa | |
| 屈服 | - | ASTM D638 | 60.0 | Mpa |
| - | ISO 527-2/5 | 60.0 | Mpa | |
| 断裂 | - | ASTM D638 | 40.0 | Mpa |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| RTI Elec | - | UL 746 | 80.0 | °C |
| RTI Imp | - | UL 746 | 80.0 | °C |
| RTI | - | UL 746 | 80.0 | °C |
| 1.8MPa,未退火,3.20mm | - | ASTM D648 | 112 | °C |
| 1.8MPa,未退火,6.40mm | - | ASTM D648 | 113 | °C |
| 1.8MPa,未退火,64.0mm跨距 | - | ISO 75-2/Af | 113 | °C |
| 流动:-40到40°C | - | ASTME831 | 4.7E-05 | cm/cm/°C |
| 23到80℃ | ISO 11359-2 | 4.9E-05 | cm/cm/°C | |
| 横向, -40到40℃ | ASTME831 | 7.1E-05 | cm/cm/°C | |
| 横向, 23到80℃ | ISO 11359-2 | 8.2E-05 | cm/cm/°C | |
| 可燃性 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| UL阻燃等级 | 1.00mm | UL 94 | V-1 | - |
| 1.50mm | UL 94 | V-0 | - | |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| -30°C | - | ASTM D256 | 42 | J/m |
| 23°C | - | ASTM D256 | 45 | J/m |
| -30°C | - | ISO 180/1A | 5.0 | kJ/m² |
| - | ISO 180/1A | 4.0 | kJ/m² | |
| 23°C | - | ISO 180/1A | 6.0 | kJ/m² |
| - | ISO 180/1A | 5.0 | kJ/m² | |
| - | ASTM D4812 | 700 | J/m | |
| - | ISO 180/1U | 57 | kJ/m² | |
| 落镖冲击 | 23°C,TotalEnergy | ASTM D3763 | 15.9 | J |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。