| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 收缩率 | MD | Internal Method | 0.38 | % |
| TD | Internal Method | 0.46 | % | |
| 24hr,50%RH | - | ASTM D570 | 0.080 | % |
| 平衡,23°C,50%RH | - | ISO 62 | 0.040 | % |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 断裂,50.0mm跨距 | - | ASTM D790 | 90.0 | Mpa |
| 断裂弯曲应变 | - | ISO 178 | 2.8 | % |
| - | ASTM D638 | 6000 | Mpa | |
| 断裂 | - | ASTM D638 | 60.0 | Mpa |
| - | ISO 527-2/5 | 62.0 | Mpa | |
| - | ASTM D638 | 1.8 | % | |
| - | ISO 527-2/5 | 1.8 | % | |
| 弯曲模量 | 50.0mm跨距 | ASTM D790 | 5300 | Mpa |
| - | ISO 178 | 105 | Mpa | |
| 屈服,50.0mm跨距 | - | ASTM D790 | 90.0 | Mpa |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 23到60℃ | ISO 11359-2 | 2.9E-05 | cm/cm/°C | |
| 横向, -40到40℃ | ASTME831 | 5.8E-05 | cm/cm/°C | |
| 横向, 23到60℃ | ISO 11359-2 | 7.4E-05 | cm/cm/°C | |
| 1.8MPa,未退火,3.20mm | - | ASTM D648 | 94.0 | °C |
| 1.8MPa,未退火,6.40mm | - | ASTM D648 | 96.0 | °C |
| 1.8MPa,未退火,64.0mm跨距 | - | ISO 75-2/Af | 96.0 | °C |
| 流动:-40到40°C | - | ASTME831 | 3.1E-05 | cm/cm/°C |
| 电气性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 表面电阻率 | - | ASTM D257 | 1.0E+3-1.0E+6 | ohms |
| 体积电阻率 | - | ASTM D257 | 1.0E+4-1.0E+6 | ohms·cm |
| StaticDecay | - | FTMS101B | 10 | msec |
| 电磁屏蔽效能 (EMI) | 1.50mm | Internal Method | 47to53 | dB |
| 3.00mm | Internal Method | 60to70 | dB | |
| 可燃性 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| UL阻燃等级 | 1.50mm | UL 94 | V-0 | - |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 简支梁缺口冲击强度 | 23°C | ISO 179/1eA | 7.6 | kJ/m² |
| -30°C | - | ASTM D256 | 44 | J/m |
| 23°C | - | ASTM D256 | 60 | J/m |
| -30°C | - | ISO 180/1A | 5.3 | kJ/m² |
| 23°C | - | ISO 180/1A | 6.0 | kJ/m² |
| -30°C | - | ASTM D4812 | 330 | J/m |
| 23°C | - | ASTM D4812 | 350 | J/m |
| -30°C | - | ISO 180/1U | 21 | kJ/m² |
| 23°C | - | ISO 180/1U | 21 | kJ/m² |
| 23°C,TotalEnergy | - | ASTM D3763 | 11.5 | J |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。