| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 表面张力 | 50.0µm | - | 52 | mN/m |
| 75.0µm | - | 52 | mN/m | |
| 100.0µm | - | 52 | mN/m | |
| 光学性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 光泽度 | 60°,50.0µm | ASTM D523 | 150 | - |
| 60°,75.0µm | ASTM D523 | 150 | - | |
| 60°,100µm | ASTM D523 | 150 | - | |
| 透射率 | 50.0µm | ASTM D1003 | 87.0 | % |
| 75.0µm | ASTM D1003 | 87.0 | % | |
| 100µm | ASTM D1003 | 87.0 | % | |
| 雾度 | 50.0µm | ASTM D1003 | 3.8 | % |
| 75.0µm | ASTM D1003 | 5.3 | % | |
| 100µm | ASTM D1003 | 9.5 | % | |
| 补充信息 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 收缩率 | MD,30min:150°C,50.0µm | Internal Method | 1.0 | % |
| SurfaceTreatment | Internal Method | Inside(Corona | - | |
| MD,30min:150°C,75.0µm | Internal Method | 1.0 | % | |
| MD,30min:150°C,100.0µm | Internal Method | 1.0 | % | |
| TD,30min:150°C,50.0µm | Internal Method | 0.50 | % | |
| TD,30min:150°C,75.0µm | Internal Method | 0.50 | % | |
| TD,30min:150°C,100.0µm | Internal Method | 0.50 | % | |
| 薄膜 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 伸长率 | TD:断裂,75µm | ASTM D882 | 120 | % |
| TD:断裂,100µm | ASTM D882 | 120 | % | |
| F | MD:50.0µm | ASTM D882 | 113 | MPa |
| MD:75.0µm | ASTM D882 | 113 | MPa | |
| MD:100.0µm | ASTM D882 | 113 | MPa | |
| TD:50.0µm | ASTM D882 | 113 | MPa | |
| TD:75.0µm | ASTM D882 | 113 | MPa | |
| TD:100.0µm | ASTM D882 | 113 | MPa | |
| 伸长率 | MD:断裂,100µm | ASTM D882 | 170 | % |
| TD:断裂,50µm | ASTM D882 | 120 | % | |
| 拉伸强度 | MD:屈服,75µm | ASTM D882 | 196 | MPa |
| MD:屈服,100µm | ASTM D882 | 196 | MPa | |
| TD:屈服,50µm | ASTM D882 | 235 | MPa | |
| TD:屈服,75µm | ASTM D882 | 216 | MPa | |
| TD:屈服,100µm | ASTM D882 | 216 | MPa | |
| 伸长率 | MD:断裂,50µm | ASTM D882 | 170 | % |
| MD:断裂,75µm | ASTM D882 | 170 | % | |
| 拉伸强度 | MD:屈服,50µm | ASTM D882 | 196 | MPa |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。