| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 密度 | - | ASTM D1505 | 0.925 | g/cm³ |
| 熔体质量流动速率 | 190°C/2.16kg | ASTM D1238 | 3.5 | g/10min |
| 光学性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 雾度 | 38.1µm,BlownFilm | ASTM D1003 | 30 | % |
| 光泽度 | 45°,12.7µm,BlownFilm | ASTM D2457 | 60 | - |
| 45°,38.1µm,BlownFilm | ASTM D2457 | 25 | - | |
| 雾度 | 12.7µm,BlownFilm | ASTM D1003 | 25 | % |
| 薄膜 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 伸长率 | Break,13µm | ASTM D882 | 500 | % |
| Break,38µm | ASTM D882 | 390 | % | |
| 拉伸应变 | Break,13µm | ASTM D882 | 630 | % |
| Break,38µm | ASTM D882 | 740 | % | |
| 落镖冲击 | 13µm,BlownFilm | ASTM D1709 | 30 | g |
| 38µm,BlownFilm | ASTM D1709 | 110 | g | |
| 埃尔曼多夫撕裂强度 | 13µm,MD | ASTM D1922 | 40 | g |
| 38µm,MD | ASTM D1922 | 100 | g | |
| 13µm,TD | ASTM D1922 | 180 | g | |
| 38µm,TD | ASTM D1922 | 220 | g | |
| 割线模量 | 13µm | ASTM D882 | 252 | MPa |
| 38µm | ASTM D882 | 307 | MPa | |
| 13µm | ASTM D882 | 255 | MPa | |
| 38µm | ASTM D882 | 314 | MPa | |
| 拉伸强度 | Break,13µm | ASTM D882 | 9.65 | MPa |
| Break,38µm | ASTM D882 | 33.1 | MPa | |
| Break,13µm | ASTM D882 | 7.24 | MPa | |
| Break,38µm | ASTM D882 | 23.4 | MPa |