| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 密度 | - | ASTM D792 | 1.84 | g/cm³ |
| 门尼粘度 | ML1+10,121°C | ASTM D1646 | 65 | MU |
| 弹性体 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 伸长率 | 断裂,23°C15 | ASTM D412 | 410 | % |
| 撕裂强度 | 150°C | ASTM D624 | 10.4 | kN/m |
| 压缩永久变形 | 200°C,22hr | ASTM D395B | 17 | % |
| 200°C,22hr18 | ASTM D395B | 14 | % | |
| 200°C,336hr | ASTM D395B | 53 | % | |
| 200°C,336hr18 | ASTM D395B | 56 | % | |
| 伸长率 | 断裂,23°C12 | ASTM D412 | 160 | % |
| 断裂,23°C13 | ASTM D412 | 320 | % | |
| 断裂,23°C14 | ASTM D412 | 310 | % | |
| 拉伸强度 | 100%应变,23°C14 | ASTM D412 | 4.30 | MPa |
| 100%应变,23°C15 | ASTM D412 | 3.50 | MPa | |
| 屈服,23°C11 | ASTM D412 | 13.5 | MPa | |
| 屈服,23°C12 | ASTM D412 | 10.1 | MPa | |
| 屈服,23°C13 | ASTM D412 | 20.4 | MPa | |
| 屈服,23°C14 | ASTM D412 | 20.8 | MPa | |
| 屈服,23°C15 | ASTM D412 | 15.7 | MPa | |
| 伸长率 | 断裂,23°C11 | ASTM D412 | 330 | % |
| 拉伸强度 | 23°C6 | ASTM D412 | 0.600 | MPa |
| 23°C7 | ASTM D412 | 0.700 | MPa | |
| 23°C8 | ASTM D412 | 0.800 | MPa | |
| 23°C9 | ASTM D412 | 0.800 | MPa | |
| 23°C10 | ASTM D412 | 1.10 | MPa | |
| 100%应变,23°C11 | ASTM D412 | 3.30 | MPa | |
| 100%应变,23°C12 | ASTM D412 | 5.10 | MPa | |
| 100%应变,23°C13 | ASTM D412 | 4.40 | MPa | |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 硬度 | 邵氏A,23°C | ASTM D2240 | 67 | - |
| 邵氏A,23°C2 | ASTM D2240 | 73 | - | |
| 邵氏A,23°C3 | ASTM D2240 | 69 | - | |
| 邵氏A,23°C4 | ASTM D2240 | 71 | - | |
| 邵氏A,23°C5 | ASTM D2240 | 70 | - | |
| 老化 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 体积变化 | 23°C,168hr,C级标准燃料 | ASTM D471 | 3.5 | % |
| 23°C,168hr,甲醇 | ASTM D471 | 55 | % | |
| 100°C,168hr,在水中 | ASTM D471 | 4.3 | % |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。