| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 密度 | -- | ASTM D792 | 0.948to1.26 | g/cm³ |
| 23°C | ISO 1183 | 1.04to1.68 | g/cm³ | |
| 熔体质量流动速率 | 230°C/2.16kg | ASTM D1238 | 4.7to21 | g/10min |
| 230°C/2.16kg | ISO 1133 | 9.6to20 | g/10min | |
| 收缩率 | MD:23°C | ASTM D955 | 0.99to1.6 | % |
| TD:23°C | ASTM D955 | 1.5to2.0 | % | |
| 23°C | ISO 294-4 | 0.70to1.1 | % | |
| 吸水率 | 23°C,24hr | ASTM D570 | 0.010to0.050 | % |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 拉伸强度 | 屈服,23°C | ISO 527-2 | 13.4to35.1 | MPa |
| 断裂,23°C | ASTM D638 | 14.9to17.3 | MPa | |
| 23°C | ASTM D638 | 22.9to32.0 | MPa | |
| 伸长率 | 屈服,23°C | ASTM D638 | 4.0to7.8 | % |
| 屈服,23°C | ISO 527-2 | 1.7to9.1 | % | |
| 断裂,23°C | ASTM D638 | 5.0to53 | % | |
| 断裂,23°C | ISO 527-2 | 2.0to59 | % | |
| 弯曲模量 | 23°C | ASTM D790 | 1370to3090 | MPa |
| 23°C | ISO 178 | 1570to4510 | MPa | |
| 弯曲强度 | 23°C | ASTM D790 | 34.6to49.2 | MPa |
| 拉伸模量 | 23°C | ASTM D638 | 1390to3100 | MPa |
| 拉伸强度 | 屈服,23°C | ASTM D638 | 17.0to33.4 | MPa |
| 弯曲强度 | 屈服,23°C | ASTM D790 | 42.2to45.1 | MPa |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 热变形温度 | 1.8MPa,未退火 | ISO 75-2/A | 48.0to70.5 | °C |
| 维卡软化温度 | -- | ASTM D1525 | 89.3to170 | °C |
| -- | ISO 306 | 85.0to156 | °C | |
| 热变形温度 | 0.45MPa,未退火 | ASTM D648 | 95.4to121 | °C |
| 0.45MPa,未退火 | ISO 75-2/B | 125 | °C | |
| 1.8MPa,未退火 | ASTM D648 | 53.8to74.6 | °C | |
| 电气性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 体积电阻率 | 23°C | ASTM D257 | 9.8E+15到1.0E+16 | ohms·cm |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 洛氏硬度 | 23°C | ASTM D785 | 85to101 | - |
| 硬度 | 23°C | ASTM D2240 | 73to75 | - |
| 23°C | ISO 868 | 67to75 | - | |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 悬臂梁缺口冲击强度 | 23°C | ASTM D256 | 25to58 | J/m |
| 23°C | ISO 180 | 1.9to4.2 | kJ/m² | |
| 悬壁梁无缺口冲击强度 | 23°C | ASTM D256 | 320to1300 | J/m |
| 23°C | ISO 180 | 4.9to12 | kJ/m² | |
| 落镖冲击 | 23°C | ASTM D3029 | 0.339to18.8 | J |
| 23°C | ASTM D5420 | 0.565to6.80 | J |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。