| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| Color | L:50.0µm | ASTM D2244 | 96 | - |
| 密度 | - | ASTM D1505 | 1.30 | g/cm³ |
| 表面张力 | HarmonicMean,Dispersive:23°C,50.0µm | - | 44 | mN/m |
| HarmonicMean,Polar:23°C,50.0µm | - | 3.0 | mN/m | |
| HarmonicMean,Total:23°C,50.0µm | - | 48 | mN/m | |
| Color | b:50.0µm | ASTM D2244 | 0.38 | - |
| 固有粘度 | 23°C,50.0µm | Internal Method | 0.70 | - |
| 23°C,250.0µm | Internal Method | 0.70 | - | |
| Color | a:50.0µm | ASTM D2244 | 0.020 | - |
| 光学性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 透射率 | 总计,50.0µm | ASTM D1003 | 92.0 | % |
| 常规,250µm | ASTM D1003 | 89.0 | % | |
| 总计,250µm | ASTM D1003 | 92.0 | % | |
| 透明度 | 50.0µm | ASTM D1746 | 98.0 | - |
| 光泽度 | 60°,50.0µm | ASTM D2457 | 110 | - |
| 60°,250µm | ASTM D2457 | 161 | - | |
| 透射率 | 常规,50.0µm | ASTM D1003 | 87.0 | % |
| 透明度 | 250µm | ASTM D1746 | 99.0 | - |
| 雾度 | 50.0µm | ASTM D1003 | 3.8 | % |
| 250µm | ASTM D1003 | 1.4 | % | |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 维卡软化温度 | - | ASTM D1525 | 69.0 | °C |
| 玻璃转化温度 | - | ASTM D1525 | 71.0 | °C |
| 补充信息 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 撕裂强度 | TD:23°C,250.0µm | ASTM D2582 | 62 | N |
| 收缩率 | 90°C,50.0µm | - | 78 | % |
| 撕裂强度 | MD:23°C,250.0µm | ASTM D2582 | 51 | N |
| 薄膜 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 薄膜厚度 | - | - | 50250 | µm |
| 割线模量 | MD:50µm | ASTM D882 | 2000 | MPa |
| MD:250µm | ASTM D882 | 1900 | MPa | |
| TD:50µm | ASTM D882 | 5300 | MPa | |
| TD:250µm | ASTM D882 | 1900 | MPa | |
| 伸长率 | TD:断裂,50µm | ASTM D882 | 42 | % |
| TD:断裂,250µm | ASTM D882 | 4.0 | % | |
| 拉伸强度 | TD:断裂,250µm | ASTM D882 | 50.0 | MPa |
| 伸长率 | MD:屈服,50µm | ASTM D882 | 3.0 | % |
| TD:屈服,50µm | ASTM D882 | 4.0 | % | |
| MD:断裂,50µm | ASTM D882 | 480 | % | |
| MD:断裂,250µm | ASTM D882 | 4.0 | % | |
| 撕裂强度 | TD:23°C,250.0µm | ASTM D1938 | 37 | kN/m |
| 埃尔曼多夫撕裂强度 | MD:50µm | ASTM D1922 | 240 | g |
| MD:250µm | ASTM D1922 | 700 | g | |
| TD:250µm | ASTM D1922 | 860 | g | |
| 氧气透过率 | 30°C,50µm,68%RH | ASTM D3985 | 3.9 | cm³·mm/m²/atm/24hr |
| 30°C,250µm,68%RH | ASTM D3985 | 7.4 | cm³·mm/m²/atm/24hr | |
| 水蒸气透过率 | 38°C,100%RH,50µm | ASTMF1249 | 25 | g/m²/24hr |
| 38°C,100%RH,250µm | ASTMF1249 | 6.7 | g/m²/24hr | |
| 撕裂强度 | MD:23°C,250.0µm | ASTM D1938 | 34 | kN/m |
| 拉伸强度 | MD:屈服,50µm | ASTM D882 | 43.0 | MPa |
| TD:屈服,50µm | ASTM D882 | 105 | MPa | |
| MD:断裂,50µm | ASTM D882 | 49.0 | MPa | |
| MD:断裂,250µm | ASTM D882 | 51.0 | MPa | |
| TD:断裂,50µm | ASTM D882 | 258 | MPa |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。