| 物性性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 吸水率 | - | ASTM D570/ISO 62 | 7.1 | % |
| 收缩率 | - | ASTM D955 | 1.2 | % |
| 密度 | - | ASTM D792/ISO 1183 | 1.22 | - |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 挤剪强度 | 23℃,DAM | ASTM D-732 | 76 | Mpa |
| 拉伸强度 | 23℃,50%RH | ASTM D-638 | 82.7 | Mpa |
| 23℃,DAM | ASTM D-638 | 103.4 | Mpa | |
| 泰伯耐磨性 | 50%RH | - | 12 | cycles |
| 弯曲强度 | 23℃,DAM | ASTM D-790 | 165 | Mpa |
| 弯曲模量 | 23℃,50%RH | ASTM D-790 | 2758 | Mpa |
| 断裂伸长率 | 23℃,50%RH | ASTM D-638 | 8 | % |
| 弯曲强度 | - | ASTM D790/ISO 178 | 165 | kg·cm/cm(J/M)ft·lb/in |
| 弯曲模量 | - | ASTM D790/ISO 178 | 4826 | kg·cm/cm(J/M)ft·lb/in |
| 拉伸强度 | - | ASTM D638/ISO 527 | 103.4 | kg/cm²(MPa)[Lb/in²] |
| 断裂伸长率 | - | ASTM D638/ISO 527 | 2 | % |
| 硬度(Rockwell M) | 50%RH | ASTM D-785 | M84 | - |
| 洛氏硬度 | 50%RH | ASTM D-785 | R113 | - |
| 悬臂梁缺口冲击强度 | 23℃,50%RH | ASTM D-256 | 53 | J/m |
| 洛氏硬度 | DAM | ASTM D-785 | R122 | - |
| 硬度(Rockwell M) | DAM | ASTM D-785 | M95 | - |
| 断裂伸长率 | 23℃,DAM | ASTM D-638 | 2 | % |
| 弯曲模量 | 23℃,DAM | ASTM D-790 | 4826 | Mpa |
| 悬臂梁缺口冲击强度 | 23℃,DAM | ASTM D-256 | 48 | J/m |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 热变形温度 | 1.8MPa | ASTM D-648 | 243 | °C |
| 线性热膨胀系数 | - | ASTM D-696 | 2.7×10 | m/m/℃ |
| 熔融温度 | DAM | ASTM D-789 | 255 | °C |
| 50%RH | ASTM D-789 | 255 | °C | |
| 线性热膨胀系数 | - | ASTM D696/ISO 11359 | 2.7×10-5 | mm/mm.℃ |
| 熔融温度 | - | - | 255 | ℃(℉) |
| 燃烧性(率) | - | UL 94 | HB | - |
| 电气性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 介电常数 | - | ASTM D150/IEC 60250 | 150 | - |
| - | ASTM D150/IEC 60250 | 130 | - | |
| 其他 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 特性 | - | - | 注塑级.高强度13%玻纤 | - |
| 基本性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 吸水率 | 饱和(23℃) | ASTM D-570 | 7.1 | % |