| 测试条件 | 测试方法 | 测试结果 | 测试单位 | |
|---|---|---|---|---|
| 拉伸强度 | 屈服 | ASTM D638 | 28.6 | MPa |
| 拉伸模量 | - | ASTM D638 | 276 | MPa |
| 硬度 | 邵氏D | ASTM D2240 | 60 | - |
| 吸水率 | 24hr | ASTM D570 | 0.030 | % |
| 密度 | - | ASTM D792 | 2.14 | g/cm³ |
| UL阻燃等级 | - | UL 94 | V-0 | - |
| 耐电弧性 | - | ASTM D495 | 180 | sec |
| 耗散因数 | 1MHz | ASTM D150 | 3E-04 | - |
| 60Hz | ASTM D150 | 2.5E-04 | - | |
| 介电常数 | 1MHz | ASTM D150 | 2.10 | - |
| 热变形温度 | 0.45MPa,未退火 | ASTM D648 | 73.3 | °C |
| 悬臂梁缺口冲击强度 | 24°C | ASTM D256 | 无断裂 | - |
| 介电常数 | 60Hz | ASTM D150 | 2.10 | - |
| 介电强度 | - | ASTM D149 | 20 | kV/mm |
| 弯曲模量 | - | ASTM D790 | 689 | MPa |
| 伸长率 | 屈服 | ASTM D638 | 330 | % |
| 体积电阻率 | - | ASTM D257 | 1E+18 | ohms·cm |
| 表面电阻率 | - | ASTM D257 | 1E+17 | ohms |
| 导热系数 | - | ASTMC177 | 0.26 | W/m/K |
| 线性热膨胀系数 | MD | ASTM D696 | 1.2E-04 | cm/cm/°C |
| 熔融温度 | - | - | 302to310 | °C |
| 脆化温度 | - | ASTM D746 | -196 | °C |
| 连续使用温度 | - | ASTM D794 | 260 | °C |
| 热变形温度 | 1.8MPa,未退火 | ASTM D648 | 47.8 | °C |