| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 密度 | - | ASTM D792 | 1.82 | g/cm³ |
| 门尼粘度 | ML1+10,121°C | ASTM D1646 | 33 | MU |
| 弹性体 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 拉伸强度 | 100%应变,23°C6 | ASTM D412 | 3.80 | MPa |
| 100%应变,23°C7 | ASTM D412 | 7.80 | MPa | |
| 100%应变,23°C8 | ASTM D412 | 7.70 | MPa | |
| 伸长率 | 断裂,23°C9 | ASTM D412 | 180 | % |
| 断裂,23°C10 | ASTM D412 | 150 | % | |
| 压缩永久变形 | 23°C,70hr | ASTM D395B | 10 | % |
| 200°C,70hr | ASTM D395B | 20 | % | |
| 232°C,22hr | ASTM D395B | 30 | % | |
| 拉伸强度 | 100%应变,23°C9 | ASTM D412 | 5.50 | MPa |
| 100%应变,23°C10 | ASTM D412 | 7.80 | MPa | |
| 屈服,23°C6 | ASTM D412 | 8.20 | MPa | |
| 屈服,23°C7 | ASTM D412 | 11.7 | MPa | |
| 屈服,23°C8 | ASTM D412 | 11.9 | MPa | |
| 屈服,23°C9 | ASTM D412 | 10.7 | MPa | |
| 屈服,23°C10 | ASTM D412 | 11.6 | MPa | |
| 伸长率 | 断裂,23°C6 | ASTM D412 | 240 | % |
| 断裂,23°C7 | ASTM D412 | 150 | % | |
| 断裂,23°C8 | ASTM D412 | 150 | % | |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 硬度 | 邵氏A,23°C4 | ASTM D2240 | 83 | - |
| 邵氏A,23°C5 | ASTM D2240 | 83 | - | |
| 邵氏A,23°C | ASTM D2240 | 79 | - | |
| 邵氏A,23°C2 | ASTM D2240 | 80 | - | |
| 邵氏A,23°C3 | ASTM D2240 | 81 | - |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。