| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 收缩率 | TD:3.20mm | ASTM D955 | 0.40-0.70 | % |
| TD:3.20mm | ISO 2577 | 0.40-0.70 | % | |
| MD:3.20mm | ISO 2577 | 0.40-0.70 | % | |
| 熔体质量流动速率 | 250°C/10.0kg | ASTM D1238 | 31 | g/10min |
| 250°C/2.16kg | ASTM D1238 | 3.0 | g/10min | |
| 250°C/10.0kg | ISO 1133 | 31 | g/10min | |
| 250°C/2.16kg | ISO 1133 | 3.0 | g/10min | |
| 收缩率 | MD:3.20mm | ASTM D955 | 0.40-0.70 | % |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 拉伸模量 | - | ASTM D638 | 1900 | Mpa |
| - | ISO 527-2/50 | 1900 | Mpa | |
| 拉伸强度 | 屈服 | ASTM D638 | 49.0 | Mpa |
| 屈服 | ISO 527-2/50 | 47.0 | Mpa | |
| 断裂 | ASTM D638 | 39.0 | Mpa | |
| 断裂 | ISO 527-2/50 | 41.0 | Mpa | |
| 伸长率 | 断裂 | ASTM D638 | 100 | % |
| 拉伸应变 | 断裂 | ISO 527-2/50 | 73 | % |
| 弯曲模量 | - | ASTM D790 | 1900 | Mpa |
| - | ISO 178 | 2000 | Mpa | |
| 弯曲强度 | - | ASTM D790 | 66.0 | Mpa |
| - | ISO 178 | 70.0 | Mpa | |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 线性热膨胀系数 | MD:40to100°C | ASTME831 | 8.5E-05 | cm/cm/°C |
| MD:40to100°C | ISO 11359-2 | 8.5E-05 | cm/cm/°C | |
| 热变形温度 | 0.45MPa,未退火,6.40mm | ASTM D648 | 120 | °C |
| 0.45MPa,Annealed,4.00mm | ISO 75-2/B | 116 | °C | |
| 1.8MPa,未退火,6.40mm | ASTM D648 | 100 | °C | |
| 1.8MPa,Annealed,4.00mm | ISO 75-2/A | 101 | °C | |
| 维卡软化温度 | -- | ISO 306/B50 | 111to113 | °C |
| -- | ISO 306/B120 | 114 | °C | |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 洛氏硬度 | R级 | ASTM D785 | 105 | - |
| R级 | ISO 2039-2 | 107 | - | |
| 冲击性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 悬臂梁缺口冲击强度 | -30°C | ISO 180/1A | 35 | kJ/m² |
| 23°C | ISO 180/1A | 45 | kJ/m² | |
| 简支梁缺口冲击强度 | 23°C | ISO 179/1eA | 47 | kJ/m² |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。