| 物理性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 横向流动 | - | ASTM D955 | 0.80 | % |
| 垂直流动方向 | - | ISO 2577 | 0.80 | % |
| 密度 | - | ASTMD792 | 1.14 | g/cm³ |
| 流动方向 | ISO 2577 | 0.80 | % | |
| 流动 | - | ASTM D955 | 0.80 | % |
| 机械性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 弯曲模量 | 23°C | ASTMD790 | 103 | MPa |
| 70°C | ASTMD790 | 34.5 | MPa | |
| 热性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 玻璃转化温度 | - | DMA | -40.0 | °C |
| 维卡软化温度 | - | ISO 306/50 | 116 | °C |
| 脆化温度 | - | ASTMD746 | <-68.0 | °C |
| 弹性体 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 拉伸强度 | 屈服 | ASTMD412 | 41.4 | MPa |
| 压缩永久变形 | 23°C,22hr | ASTMD395B | 22 | % |
| 70°C,22hr3 | ASTMD395B | 40 | % | |
| 70°C,22hr | ASTMD395B | 75 | % | |
| 硬度 | - | ASTM D2632 | 35 | % |
| 伸长率 | 断裂 | ASTMD412 | 400 | % |
| 压缩永久变形 | 23°C,22hr2 | ASTMD395B | 20 | % |
| 硬度 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 硬度 | 邵氏D | ASTMD2240 | 45 | - |
| 补充信息 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| CompressiveLoad | 25%Deflection | ASTM D575 | 8.38 | MPa |
| 5%Deflection | ASTM D575 | 2.10 | MPa | |
| 50%Deflection | ASTM D575 | 21.5 | MPa | |
| 2%Deflection | ASTM D575 | 0.896 | MPa | |
| 20%Deflection | ASTM D575 | 6.89 | MPa | |
| 10%Deflection | ASTM D575 | 3.79 | MPa | |
| 15%Deflection | ASTM D575 | 5.34 | MPa | |
| 老化 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 空气中极限伸长率的变化率 | 100°C,70hr | ASTMD573 | 9.0 | % |
| 100°C,168hr | ASTMD573 | 14 | % | |
| 100°C,336hr | ASTMD573 | 13 | % | |
| 100°C,504hr | ASTMD573 | 17 | % | |
| 空气中硬度(Shore)的变化率 | 支撐D,100°C,70hr | ASTMD573 | -1.0 | - |
| 支撐D,100°C,168hr | ASTMD573 | 0.0 | - | |
| 支撐D | - | ASTMD471 | -6.0 | - |
| - | ASTM D471 | -1.0 | - | |
| - | ASTM D471 | -1.0 | - | |
| - | ASTM D471 | -4.0 | - | |
| - | ASTM D471 | 2.0 | - | |
| - | ISO 175 | -1.0 | - | |
| - | ISO 175 | -1.0 | - | |
| - | ISO 175 | 0.0 | - | |
| - | ISO 175 | -1.0 | - | |
| - | ISO 175 | -1.0 | - | |
| - | ISO 175 | -4.0 | - | |
| - | ASTMD471 | -6.0 | - | |
| - | ASTM D471 | -1.0 | - | |
| - | ASTMD471 | -5.0 | - | |
| - | ASTM D471 | -1.0 | - | |
| - | ASTMD471 | -7.0 | - | |
| - | ASTM D471 | 0.0 | - | |
| - | ASTM D471 | -4.0 | - | |
| - | ASTM D471 | -1.0 | - | |
| - | ASTM D471 | -4.0 | - | |
| - | ASTM D471 | 0.0 | - | |
| - | ASTM D471 | -4.0 | - | |
| 空气中硬度(Shore)的变化率 | 支撐D,100°C,336hr | ASTMD573 | -1.0 | - |
| 支撐D,100°C,504hr | ASTMD573 | 0.0 | - | |
| 支撐D | - | ISO 175 | 2.0 | - |
| - | ISO 175 | -4.0 | - | |
| - | ISO 175 | -1.0 | - | |
| - | ISO 175 | -4.0 | - | |
| - | ISO 175 | 0.0 | - | |
| - | ISO 175 | -4.0 | - |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。