| 测试条件 | 测试方法 | 测试结果 | 测试单位 | |
|---|---|---|---|---|
| 极限氧指数 | - | ASTM D2863 | 52 | % |
| 介电常数 | 23°C | ASTM D150 | 2.57 | - |
| 摩擦系数 | - | ASTM D1894 | 0.20 | - |
| 弯曲强度 | 23°C | ASTM D790 | 47.0 | MPa |
| 洛氏硬度 | 23°C | ASTM D785 | 90 | - |
| 熔体质量流动速率 | 275°C/2.16kg | ASTM D1238 | 1.0to25 | g/10min |
| 密度 | - | ASTM D792 | 1.68 | g/cm³ |
| 结晶峰温度 | DSC | ASTM D3418 | 222to223 | °C |
| 熔融温度 | - | - | 225to242 | °C |
| 脆化温度 | - | ASTM D746 | -76.1--73.7 | °C |
| 热变形温度 | 1.8MPa,未退火 | ASTM D648 | 64.9to65.2 | °C |
| 0.45MPa,未退火 | ASTM D648 | 90.0to90.6 | °C | |
| 伸长率 | 屈服,23°C | ASTM D638 | 5.0to9.9 | % |
| 拉伸强度 | 断裂,23°C | ASTM D638 | 46.5to54.0 | MPa |
| 屈服,23°C | ASTM D638 | 29.6to30.1 | MPa | |
| 拉伸模量 | 23°C | ASTM D638 | 1650to1660 | MPa |
| 硬度 | 23°C | ASTM D2240 | 75 | - |
| 介电强度 | 23°C | ASTM D149 | 14to19 | kV/mm |
| 体积电阻率 | 23°C | ASTM D257 | 5.4E+16到5.5E+16 | ohms·cm |
| 线性热膨胀系数 | MD | ASTM D696 | 1E-04 | cm/cm/°C |
| 弯曲模量 | 23°C | ASTM D790 | 1690 | MPa |
| 伸长率 | 断裂,23°C | ASTM D638 | 240to250 | % |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。