| 测试条件 | 测试方法 | 测试结果 | 测试单位 | |
|---|---|---|---|---|
| 密度 | - | ISO 1183 | 1.15 | g/cm³ |
| 熔体质量流动速率 | 190°C/2.16kg | ISO 1133 | 0.40 | g/10min |
| 吸水率 | 70°C | IEC 60811-1-3 | 0.110 | mg/cm² |
| 拉伸强度 | Yield | IEC 60811-1-1 | 11.0 | MPa |
| 拉伸应变 | Break | IEC 60811-1-1 | 400 | % |
| 弯曲模量 | - | ISO 178 | 205 | MPa |
| 硬度 | ShoreD,15sec | ISO 868 | 39 | - |
| ColdBend | -40°C | IEC 60811-1-4 | Pass | - |
| ColdImpact | -40°C | IEC 60811-1-4 | Pass | - |
| 空气中拉伸强度的变化率 | --7 | ISO 1817 | >-80 | % |
| 100°C,240hr6 | IEC 60811-1-2 | >-80 | % | |
| 体积电阻率 | - | IEC 60093 | 4.5E+16 | ohms·cm |
| ConeCalorimeter | HeatCombustion11 | ISO 5660 | 29.0 | - |
| Ignitiontime9 | ISO 5660 | 2.6 | min | |
| MaxHeatRelease9 | ISO 5660 | 282 | kW/m² | |
| SmokeObscuration12 | ISO 5660 | 506 | - | |
| Corrosion-ofCombustionFumes | - | IEC 60754-2 | 1.50 | µS/cm |
| 耐压强度 | 90°C | IEC 60811-3-1 | 9.0 | % |
| 介电强度 | - | IEC 60243-1 | 20 | kV/mm |
| 极限氧指数 (LOI) | - | ISO 4589-2 | 31 | % |
| BreakdownDuration | - | IEC 60227-2/2.3 | Pass | - |
| 击穿电压强度 | - | ISO 6722 | 40000 | V |
| ConeCalorimeter | AverageHeatRelease9 | ISO 5660 | 175 | kW/m² |
| CO9 | ISO 5660 | 0.0140 | kg/m³ | |
| CO210 | ISO 5660 | 1.85 | kg/m³ |