| 光学性能 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
|---|---|---|---|---|
| 光泽度 | 60° | ASTM D2457 | 20 | - |
| 雾度 | - | ASTM D1003 | 56 | % |
| 薄膜 | 测试条件 | 测试方法 | 测试结果 | 测试单位 |
| 薄膜厚度 | - | - | 1.0;1.15;1.25;1.5;2.0;2.5;3.0mil(25;29;32;38;51;64;76µ | - |
| 割线模量 | 1%正割,MD | ASTM D882 | 2480 | Mpa |
| 1%正割,TD | ASTM D882 | 2550 | Mpa | |
| 用量 | 31.8µm | ASTM D4321 | 30.0 | m²/kg |
| 38.1µm | ASTM D4321 | 25.0 | m²/kg | |
| 50.8µm | ASTM D4321 | 18.9 | m²/kg | |
| 63.5µm | ASTM D4321 | 15.2 | m²/kg | |
| 76.2µm | ASTM D4321 | 12.6 | m²/kg | |
| 拉伸强度 | MD:屈服 | ASTM D882 | 55.8 | Mpa |
| TD:屈服 | ASTM D882 | 55.8 | Mpa | |
| 伸长率 | MD:断裂 | ASTM D882 | 70 | % |
| TD:断裂 | ASTM D882 | 90 | % | |
| 落镖冲击 | - | ASTM D1709 | 200 | g |
| 埃尔曼多夫抗撕强度-TD | 25µm | ASTM D1922 | 7.0 | g |
| 拉伸模量 | MD:135°C | Internal Method | 1.21 | Mpa |
| TD:135°C | Internal Method | 0.896 | Mpa | |
| 用量 | 25.4µm | ASTM D4321 | 38.0 | m²/kg |
| 29.2µm | ASTM D4321 | 33.0 | m²/kg |
普拉司网尽最大努力确保此数据的准确性,但是普拉司网对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。